HDPE Property | Unit | Typical Value |
Mass density | g/cm 3 | 0.958 |
Melt flow Rate(190 centidegree /2.16kg) | g/10min | 18 |
Tensile yield strength | MPa | 27.5 |
ESCR | H | 2 |
Elongation@ break | % | 40 |
IZOD | J/m | 19.6 |
Dielectric Constant | 100KHZ | 2.32 |
1MHZ | 2.31 | |
Loss Tangent | 100KHZ | MAX 0.0001 |
1MHZ | MAX 0.0001 | |
Volume resistivity | OHM-CM | MIN 1x10 15 |
em /Film Grade | Test condition | Test Method | Value | Unit |
Density | ISO 1183 | 0.944-0.955 | g/cm3 | |
MFR | 190°C/2.16kg | ISO 1133 | 0.03-0.07 | g/10min |
Tensile strength at yield | ISO 527-2 | 22 | MPa | |
Elongation at break | ISO 527-2 | >350 | % | |
ESCR | F50,50°C,100% | ASTM D-1693A | 1000 | h |
VICAT | ASTM D-1525 | 126 | °C |